Disclosure: This post contains affiliate links and I will be compensated if you make a purchase after clicking through my links. Learn More
Stick welding, or Shielded Metal Arc Welding (SMAW), is popular for its simplicity and ability to work on many metals. But one common problem welders face is burn through. This happens when the electrode melts a hole in the workpiece, ruining the weld and the material. Burn through is frustrating, especially for beginners, but even experienced welders face it when working with thin metals or using the wrong settings. Stopping burn through is possible if you know what causes it and use the right techniques.
This article explains how to prevent burn through when stick welding. It covers everything from understanding why burn through happens, to choosing the right equipment, adjusting your settings, and using better techniques. You’ll also find practical examples, mistakes to avoid, and answers to common questions.
Whether you’re a hobbyist or a professional, you’ll learn how to get better results and save time, materials, and money.
What Causes Burn Through In Stick Welding?
Burn through occurs when the metal under the arc gets too hot and melts away, creating a hole. Understanding why this happens is key to preventing it. There are several main causes:
- Too much heat – Using high amperage or a hot electrode can quickly overheat thin metal.
- Slow travel speed – Keeping the arc in one spot for too long concentrates heat, causing holes.
- Wrong electrode – Thick or high-penetration electrodes produce more heat.
- Thin workpieces – Thin metal is more sensitive to excess heat, making burn through common.
- Poor fit-up – Large gaps between pieces cause more heat to collect in one spot.
These factors often work together. For example, using the wrong electrode on thin steel with high amperage almost always leads to burn through. Being aware of these dangers helps you adjust your technique.
How To Choose The Right Equipment
Your equipment choices have a big impact on burn through. Picking the right machine, electrode, and settings helps you control heat and avoid problems.
Stick Welding Machine
Choose a welding machine that lets you adjust the amperage in small steps. Machines with fine control are better for thin metal. Some modern inverters offer better arc stability at low amps, which helps reduce burn through.
Electrode Selection
The electrode (or “rod”) you use affects how much heat goes into the metal. For thin metal, use low-penetration, small-diameter electrodes.
- E6013 is a good choice. It runs at lower amps and produces a softer arc.
- E7014 is also suitable for thin sections.
- Use 3/32 inch (2.4 mm) or smaller electrodes for metal under 1/8 inch (3 mm) thick.
Thicker electrodes put more heat into the workpiece and are more likely to cause burn through, especially on sheet metal.
Electrode Coating
The coating on the electrode affects arc stability and heat input. For thin metal, electrodes with a rutile (titania) coating, like E6013, work well. They create a smooth, easy-to-control arc and are less likely to overheat the base metal.
Machine Settings
Check if your machine has a “hot start” feature. This increases the current for starting the arc but can also cause burn through if not adjusted. If possible, turn this feature off or reduce it when welding thin metal.

Credit: unimig.com.au
Setting The Right Amperage
Amperage is the main factor that controls heat. Too much amperage causes burn through, while too little gives poor fusion or a sticking electrode. You must set the amperage to match your electrode and workpiece thickness.
General Amperage Guidelines
The following table shows suggested amperage ranges for common electrode sizes on thin steel:
| Electrode Size | Recommended Amperage | Metal Thickness |
|---|---|---|
| 1/16″ (1.6 mm) | 20–40 A | Up to 1/16″ (1.6 mm) |
| 5/64″ (2 mm) | 30–50 A | Up to 3/32″ (2.4 mm) |
| 3/32″ (2.4 mm) | 40–90 A | 1/16″–1/8″ (1.6–3 mm) |
Start at the lower end of the range. If you see undercut or burn through, lower the amps. If the electrode sticks or the bead is tall, raise the amps slowly.
How To Test Your Settings
Before welding the actual parts, do a test weld on scrap material of the same thickness. Watch for:
- Holes or excessive melting (too hot)
- Electrode sticking or poor fusion (too cold)
- Bead shape – it should be flat, not sunken
Small changes (5–10 amps) can make a big difference.
Preparing The Workpiece
Preparation affects how the metal responds to heat. Clean, well-fitted parts reduce the chance of burn through.
Clean The Metal
Remove rust, oil, paint, and dirt from the weld area. Contaminants can cause arc instability, making it hard to control heat. Use a wire brush or grinder for best results.
Fit-up And Gaps
Poor fit-up with large gaps means the arc has to “jump” across, concentrating heat and causing burn through. Make sure the parts fit closely together.
- For sheet metal, a gap under 1/32 inch (0.8 mm) is best.
- Use clamps or magnets to hold pieces tight.
Backing Bars
A backing bar is a piece of copper or aluminum clamped behind the weld joint. It absorbs extra heat and supports the molten metal, preventing holes.
- Copper works best because it does not fuse with steel.
- Water-cooled copper backing bars are used for production welding, but a simple solid copper bar helps in the home shop.
Using a backing bar is one of the most effective ways to stop burn through on thin metal.

Credit: weldguru.com
Welding Techniques To Prevent Burn Through
Technique plays a big role in controlling heat during stick welding. How you move the electrode, the angle, and the speed all affect results.
Travel Speed
Move the electrode steadily and fast enough to avoid overheating one spot. If you pause too long, the metal will melt through. Practice keeping a constant speed.
- For thin metal, move at least 1 inch (25 mm) every 2–3 seconds.
- If you see the puddle getting too large, speed up.
Short Arc Length
Keep the arc length short. A long arc increases voltage and heat input, raising the risk of burn through.
- Hold the electrode 1/16 to 1/8 inch (1.6–3 mm) from the surface.
- If the arc “hisses” or “pops,” it’s too long.
Electrode Angle
For butt joints on sheet metal, hold the electrode at a 10–20° angle (push or drag, depending on rod type). A shallow angle helps spread the heat along the joint.
Weaving Vs. Straight Bead
Do not use wide weave patterns on thin metal. A straight bead or a very small weave is safer.
- Weaving adds more heat and increases burn through risk.
- For better control, use a “stitch” or “skip” technique.
Stitch Welding
Instead of running a long bead, weld short sections (½–1 inch), then move to another spot. This gives the metal time to cool between passes.
- Stitching is useful for lap or butt joints in sheet metal.
- After completing stitches, connect them with more short beads.
Skip Welding
Weld in one spot, then skip ahead and weld another section. Finish the skipped areas after the metal cools. This spreads the heat and lowers the risk of burn through.
Backstep Welding
Start each weld segment by moving the electrode away from the finished bead, then weld back toward the previous section. This also spreads heat.
These techniques are especially helpful when welding car panels, roofing, or thin boxes.
Managing Heat Input
Controlling total heat input is critical. Along with amperage and speed, use these tricks to help.
Use Shorter Welds
Short welds put less heat into the part. If a long seam is needed, weld in steps, allowing time for cooling.
Pause Between Passes
Let the metal cool for 30–60 seconds between welds. This prevents heat from building up and causing burn through on the next pass.
Use A Heat Sink
A heat sink is a piece of metal (usually aluminum or copper) placed behind the joint. It absorbs extra heat and supports the molten pool.
- For car bodywork, clamp an aluminum flat bar behind the seam.
- For pipes, insert a copper slug inside before welding.
This trick works well for repairs and is often used in automotive and HVAC welding.
Control The Work Environment
Wind, drafts, or cold temperatures can change how heat builds up in the workpiece. Try to weld in a controlled environment.
- Shield the work area from wind.
- If the metal is very cold, preheat it slightly with a torch or heat gun to reduce shock.
Choosing The Right Joint Design
The way you prepare and arrange the pieces affects heat control.
Butt Joints
For thin sheet metal, use a tight butt joint with no gap. If a gap is needed, keep it as small as possible.
Lap Joints
Lap joints are easier to weld without burn through because the two layers absorb more heat. Use a short stitch or skip technique.
Edge Joints
Edge joints are difficult on thin metal. Use a backing bar or heat sink to support the molten pool.
Flanged Joints
Adding a flange (a bend along the edge) increases thickness at the weld, making burn through less likely. This method is common in auto body repair.
| Joint Type | Burn Through Risk | Best Technique |
|---|---|---|
| Butt | High | Short beads, backing bar |
| Lap | Medium | Stitch, skip |
| Edge | Very High | Heat sink, short arc |
| Flanged | Low | Continuous, small beads |
Common Mistakes That Lead To Burn Through
Knowing what not to do is as important as knowing the right steps. Here are some mistakes that often cause burn through:
- Using thick electrodes – More heat goes into the workpiece.
- Ignoring amperage settings – Setting amps too high for the metal.
- Pausing too long – Stopping in one place overheats the metal.
- Welding over large gaps – Gaps focus the arc in one spot, causing holes.
- Welding dirty metal – Contaminants create unstable arc and more heat.
- Long arc length – Raises voltage and heat input.
- Wide weave beads – Increase time and heat in one area.
- No cooling time – Welding long beads without breaks.
Avoiding these mistakes is often enough to prevent most burn through problems.

Credit: weldguru.com
Advanced Tips And Non-obvious Insights
Some factors are easy to miss, especially for new welders. Here are two valuable insights:
1. Electrode Storage Matters
Electrodes that absorb moisture may cause unstable arcs, leading you to compensate with higher amperage. Store electrodes in a dry, heated container if possible. Moist rods also create more spatter, which affects bead shape and heat control.
2. Workpiece Support And Clamping
Supporting the workpiece with clamps or fixtures reduces vibration and movement during welding. If the metal moves, the arc can pause accidentally, increasing heat in one spot and causing burn through.
Examples: Preventing Burn Through In Real Situations
Let’s look at two practical examples.
Example 1: Repairing A Car Body Panel
Car body panels are usually 0. 8–1. 2 mm thick steel. Stick welding these can be tricky.
- Use E6013, 1/16″ or 5/64″ rod at 25–40 amps.
- Prepare a tight butt joint or small lap.
- Clamp a copper bar behind the seam.
- Stitch weld short beads, moving around to let the panel cool.
- Grind and finish the weld.
Example 2: Welding Hvac Sheet Metal
Galvanized ducting is 1–1. 5 mm thick.
- Use E6013, 3/32″ rod at 40–50 amps.
- Clean the zinc coating from the weld area (wear a mask).
- Use lap joints for more strength.
- Move quickly and avoid pausing.
- Use a heat sink if possible.
Both examples show how correct settings, technique, and support prevent burn through.
Comparing Stick Welding With Other Processes
Stick welding is not always the best method for thin metal. Here’s a quick comparison:
| Process | Thin Metal Performance | Burn Through Risk | Control |
|---|---|---|---|
| Stick (SMAW) | Fair | High | Moderate |
| MIG (GMAW) | Good | Medium | High |
| TIG (GTAW) | Excellent | Low | Very High |
For very thin sheet metal, TIG welding is often preferred because it gives more control. MIG welding is also easier for beginners. But with the right steps, stick welding works well for many jobs.
How To Fix Burn Through If It Happens
Even with care, burn through can still occur. You can often fix small holes.
- Let the area cool completely.
- Grind the edges of the hole to clean metal.
- Place a copper backing bar behind the hole.
- Set the machine to a lower amperage.
- Use a small-diameter electrode.
- Weld around the edge of the hole in short bursts, allowing cooling between tacks.
- Fill the hole bit by bit, connecting the tacks.
This patching method works for small holes in steel. For larger holes, cut a patch and weld it in place.
Maintenance And Safety Practices
Safe welding prevents accidents and protects your work and health.
- Always wear welding gloves, a jacket, and a helmet with the correct lens shade.
- Work in a well-ventilated area, especially when welding galvanized steel.
- Keep a fire extinguisher nearby.
- Store electrodes in a dry place to avoid moisture problems.
- Check cables and connections before each session for safety.
Proper safety helps you focus on technique and get better results.
Frequently Asked Questions
Why Does Burn Through Happen More On Thin Metal?
Thin metal heats up and melts faster because it has less material to absorb heat. Even a slight increase in amperage or a slow travel speed can cause holes. That’s why thin sheet metal is the most difficult to weld without burn through.
Can I Use Stick Welding For Car Body Repairs?
Yes, but you need to use small-diameter electrodes (1/16″ or 5/64″), low amperage, and a backing bar. Stitch welding is recommended. MIG or TIG welding is easier for car panels, but stick welding works if you use the right steps.
What’s The Best Electrode For Preventing Burn Through?
E6013 is the most common stick electrode for thin metal. It runs at low amperage, gives a soft arc, and is easy to control. Choose 1/16″ or 3/32″ sizes for best results.
How Do I Know If My Settings Are Right To Avoid Burn Through?
Test your settings on scrap metal. If you see the metal glow, sag, or form a hole, lower the amps. The bead should be flat and not sunken. If the rod sticks, raise the amps slightly.
Is There A Way To Fix A Burn Through Hole?
Yes. Use a copper backing bar behind the hole, lower the amperage, and weld short tacks around the edge. Fill the hole in small steps, letting it cool between welds. Grind and finish as needed.
—
Burn through is a common problem in stick welding, but it doesn’t have to ruin your project. With the right equipment, settings, technique, and a few expert tricks, you can weld thin metal without holes or wasted material. Always test on scrap, move quickly, and use heat sinks or backing bars for best results. With practice and attention, you’ll soon weld confidently and cleanly. For more on welding basics and safety, you can visit the Wikipedia: Shielded Metal Arc Welding page. Stick welding is a skill worth mastering, and preventing burn through is a big step toward better, stronger welds.